How Do You Run a Stress Relief Anneal?

A furnace cycle is not one temperature, although many shops treat it that way. Stress relief annealing runs on five nodes, and each node carries its own parameter and its own failure. Jiangsu Zhongtong Weiye Special Steel Co., Ltd. walks that curve below, using a non-oriented electrical steel sheet as the example.

The Short Answer

Ramp slowly, soak until the centre reaches temperature, cool slowly, unload cool, then check. The set point near 750 to 800 degrees matters less than the schedule. The schedule carries the gradient, and the gradient decides the warp. Hence two shops with the same set point can produce different results. The decision note covers whether to run the cycle at all.

Node One — The Ramp

A stack heats from the outside in, so the centre lags the surface by hours, as the heat path shows. A fast ramp therefore lifts the skin to set point, while the middle sits far below. That gradient bends a core, and it hides an incomplete soak. Hence the ramp rate follows stack mass, rather than a table. Slow wins, because patience is cheaper than a rebuild.

Node Two — The Soak

The soak must last until the coldest point arrives, and that point sits mid stack. A thermocouple on the surface therefore reports a false success, because the surface leads. A second couple buried in the load settles it, and that costs one probe. Hence soak time follows build height, not a printed rule. Short soaks leave stress in the middle, where no one measures.

Node Three — The Cool

Cooling carries as much risk as heating, since the gradient returns in reverse. A fast cool warps a stack, and it locks a fresh stress pattern into the sheets. A slow cool near 100 degrees per hour holds flatness, even though it lengthens the cycle. Therefore, the cooling branch belongs in planning, rather than in leftover time.

Node Four — The Unload

Unloading hot invites oxidation, because fresh metal meets air at temperature. That oxide spoils interlamination resistance, so a core unloaded early loses what the furnace gave, as the rust note explains. A cool unload costs hours, although it protects the surface. Hence the ramp down deserves a written rule.

Node Five — The Check

Three checks close the cycle, and they cost little. A sample cut from the load confirms recovery, since a number beats an impression. Flatness comes next, because a warped stack ruins the build. The resistance check closes, since heat may have damaged the film. Hence the list is short, and it fits beside the furnace.

Stack with a thermocouple buried in the middle

What the Atmosphere Does

Atmosphere decides surface condition rather than loss, and two options dominate. Air leaves an oxide that harms insulation, although a protective gas keeps the surface bright. A wet hydrogen atmosphere belongs to the mill, since it decarburises, so a shop cannot reproduce it. Therefore, a shop should specify bright, and leave chemistry to the line.

How the Load Is Held

Clamping decides flatness, because a loose stack relaxes into whatever shape gravity prefers. A flat plate above and below spreads the load, while a weight on top holds sheets level. Hence a shop that skips the plate saves ten minutes, then loses a build. The burr note covers the edge beside that plate.

A Schedule That Fits One Shift

Take a 10 tonne load and a ramp of 50 degrees per hour. The climb to 750 then takes about 15 hours. A soak of four hours follows, since the middle needs that long. Cooling at 100 degrees per hour from 750 down to 100 takes another six and a half hours. The whole cycle therefore runs near 26 hours, which no single shift covers. Hence a furnace plan belongs to a weekly schedule.

What Goes Wrong

One buyer trusts a surface couple, then cuts the soak short. Another cools in still air, so a warp appears across the stack. A third unloads at 300 degrees, and resistance drops with the oxide. Those three errors arrive monthly.

What We Do Not Do

We do not melt or roll steel. We do not run a customer’s furnace, because the load belongs to the stamper. Nor do we promise recovery from a set point alone.

Those limits keep the answer honest, and they keep a cycle repeatable.

Specify Your Order

Give the stack mass, the build height, the coating family, and the target loss. Those four fields then set the ramp and soak. Add the furnace type, because batch loads and coil loads follow different schedules. A grain oriented sheet covers a texture sensitive duty. A cut core arrives when the stack is built. That reply usually takes a day.

Related Reading

The stacking note covers the build after the cycle. The heat note sets the upper limit. A hub page answers six basic questions.

Frequently Asked Questions

What set point should I use?

750 to 800 degrees, and never above 850, since grain growth starts there.

How long is the soak?

Until the centre reaches temperature, which follows build height.

Why cool slowly?

Because the same gradient returns, so a fast cool warps.

Can I unload warm?

No, since surface oxidation ruins resistance before the next step.

Does atmosphere change loss?

Rarely, although it changes the surface and the resistance.

  • Email: vera.liang@ztwysteel.com
  • Location: Xishan District, Wuxi, Jiangsu, China
  • Supply range: CRGO and CRNGO 0.20–0.65 mm, four coating classes
  • Slitting: 20–1,250 mm, ±0.05 mm, burr under 0.02 mm
  • Documentation: MTC EN 10204 3.1 with grade, thickness and loss basis, 3.2 on request