Chemical Composition of Silicon Steel Sheets

A composition table is not a list of ingredients, since every line carries a floor and a ceiling. Chemical composition of silicon steel reads as two-sided limits, and one element flips between the two families. Jiangsu Zhongtong Weiye Special Steel Co., Ltd. quotes the silicon steel sheet chemistry on the certificate, so the limits travel with the coil.

The Short Answer

Iron takes the balance, and silicon runs 0.5 to 3.2 percent in non-oriented grades. Carbon, sulphur, nitrogen, oxygen, and titanium sit at a few thousandths, since each one hurts the loss. Aluminium and manganese then serve the process. Hence the table is short, and every line has a reason.

Silicon — A Floor and a Ceiling

Silicon raises resistivity, so a floor near 0.5 percent keeps the loss reachable. A ceiling near 3.2 percent keeps the sheet rollable, since brittleness rises with the alloy. An oriented grade pushes toward 2.9 to 3.3 percent, where the loss is lowest on a CRGO sheet. Therefore, the silicon line trades magnet against mill.

Aluminium — Control and Cleanliness

Aluminium refines the grain in non-oriented sheet, and it runs from about 0.2 to 0.9 percent. Too little leaves a coarse grain after annealing, so the hysteresis loss rises. Too much invites alumina inclusions, and a casting defect follows. In the oriented route it also forms a nitride inhibitor, so the anneal sets the limit. Hence this line serves the process first.

Carbon — A Ceiling Only

Carbon has no floor, since zero would be ideal and about 0.003 percent is practical. Carbon sits in solid solution and ages the sheet, so the loss drifts upward over months. A wet anneal removes it, and a mill that skips that step ships a sheet with a moving loss figure. Therefore, carbon is the one line that only points down.

Sulphur — The Element That Flips

In a non-oriented grade, sulphur stays under 0.005 percent, since a sulphide inclusion pins the grain. In an oriented route, sulphur sits near 0.01 to 0.03 percent, because manganese sulphide acts as an inhibitor. That inhibitor lets the mill grow one favoured orientation, and the sheet then loses less along the roll. Hence the same element helps one family and hurts the other.

Nitrogen — The Same Flip

Nitrogen follows sulphur, since aluminium nitride plays the inhibitor role in the oriented route. A few thousandths of nitrogen then hold the grain during the high-temperature anneal. In a non-oriented grade the same nitrogen pins the grain, so the limit drops to 0.003 percent. Therefore, a chemistry sheet must state the family before the limit.

Manganese — Tying Up Sulphur

Manganese sits near 0.1 to 0.5 percent, and it combines with sulphur before that sulphur hurts the grain. Too little leaves free sulphur, and hot shortness follows at the mill. Too much raises the inclusion volume, and the loss creeps up. Hence manganese is a buffer, not a magnet element.

Chemical composition certificate for a silicon steel coil

Phosphorus and Titanium

Phosphorus stays low in most grades, since it embrittles a thin sheet, yet a small addition raises resistivity. Titanium stays under about 0.003 percent, since titanium nitride pins the grain and blocks growth. Oxygen also stays low, since an oxide inclusion does the same. Therefore, three minor lines protect one property.

Reading the Balance

A certificate lists iron as the balance, so the lines never sum to 100 percent. A 3 percent grade then carries about 96 percent iron and a trace of everything else. Buyers who add the lines and expect 100 percent misread the sheet. Hence the word balance carries the rest.

Tolerance Against Typical

A certificate gives a maximum for each element, and a heat report gives a typical value. A 0.003 percent carbon limit allows a heat at 0.001 percent, and both pass. Buyers who compare certificates should compare maxima first, then typicals. Therefore, a limit and a reading are different numbers.

What Changes With Thickness

A thin gauge holds the same chemistry, since the alloy does not change with the roll. Its carbon limit tightens in practice, since a thin section ages faster at temperature. A 0.23 mm oriented sheet therefore needs a cleaner heat than a 0.35 mm sheet. Hence gauge and cleanliness travel together.

Where Buyers Get It Wrong

A buyer compares two grades by silicon alone and ignores the carbon limit. Another applies a non-oriented sulphur limit to an oriented coil and rejects a good heat. A third adds the lines and expects 100 percent. Those three errors cover most of our returns.

What We Do Not Do

We do not melt or roll steel. We do not alter a heat report. Nor do we accept a chemistry that the mill did not certify.

Those limits keep the table honest.

Specify Your Order

First, name the family and the grade. Second, state the thickness and the loss figure. Then ask for the chemistry limits, so the certificate matches the anneal you plan.

Related Reading

The grade naming note explains how a loss code is read, so a 23P85 sits beside a 50W470. The applications note maps grades onto machines, since a transformer and a motor tolerate different chemistry.

Frequently Asked Questions

What is silicon steel made of? Iron with 0.5 to 3.2 percent silicon, plus process elements.

Why is carbon capped? Carbon ages the sheet and raises the loss.

Is sulphur always harmful? No, an oriented route uses it as an inhibitor.

Does aluminium change the magnet? It mainly controls the grain, and it forms a nitride inhibitor.

Why does iron show as balance? The other lines are small, so iron fills the rest.

  • Email: vera.liang@ztwysteel.com
  • Location: Xishan District, Wuxi, Jiangsu, China
  • Supply range: CRGO and CRNGO 0.23–0.65 mm, chemistry on certificate
  • Slitting: 20–1,250 mm, ±0.05 mm, burr under 0.02 mm
  • Documentation: MTC EN 10204 3.1 with heat chemistry and loss figure, 3.2 on request