What are the different grades of silicon steel?

Grades of silicon steel arrange themselves into four families, and each family answers a different magnetic job. In practice, the code on the certificate tells you gauge and loss, while the family tells you texture and process. Consequently, reading both avoids expensive mismatches. Jiangsu Zhongtong Weiye Special Steel Co., Ltd. quotes by code and basis.

The Family Tree in One View

  • Branch A — grain-oriented: directional sheet for transformers.
  • Branch B — non-oriented: isotropic sheet for motors and reactors.
  • Branch C — semi-processed: sheet that needs a customer anneal.
  • Branch D — specialty: very thin or very high-silicon sheet.

Each branch splits again by loss class, so the tree stays useful at quotation time.

Branch A — Grain-Oriented

Oriented grades carry codes such as 23P85, 27P100, 27P110, and 30P120. The number before the letter gives gauge in hundredths of a millimetre, and the number after gives loss in W/kg at 1.7 T and 50 Hz.

Within this branch, three tiers exist. Conventional grades reach moderate loss, Hi-B grades improve texture, and domain-refined grades add laser scribing for the lowest loss. Therefore, a 23P85 core beats a 30P120 core on no-load loss, at a price.

Branch B — Non-Oriented

Non-oriented grades carry codes such as 35W230, 50W470, 50W600, and 65W1300. Here the loss figure is measured at 1.5 T and 50 Hz, since motors rarely push beyond that.

Older AISI labels coexist, including M15, M19, M27, M36, M43, and M47. Those letters mark families rather than a loss number, so never convert them by intuition. Compare the stated W/kg instead.

Appliance cores, such as a silicon steel coiled magnet ring for washer motors, usually sit in the cheaper half of this branch.

Branch C — Semi-Processed

Semi-processed sheet ships without final annealing, and the customer anneals after stamping. Consequently, the mill saves energy and the buyer gains formability. Small motors and ballasts used this route heavily, and it survives in cost-driven designs. Its drawback is dependence on your furnace, since annealing error becomes your problem.

Branch D — Specialty

Two specialty lines matter commercially. Very thin sheet at 0.20 mm serves high-frequency duty, while high-silicon sheet near 4.5–6.5% trades saturation for resistivity. Neither suits general work, and both cost more per kilo.

How to Read a Code

  1. Gauge sits in the leading digits, usually 23 to 65.
  2. Loss sits in the trailing digits, quoted at a fixed induction.
  3. The letter marks the family, P for oriented and W for non-oriented.
  4. The standard, EN 10106, EN 10107, JIS C2552, or ASTM A677, fixes the test method.

Hence a complete specification names all four items, not just the code.

Five Traps in Grade Selection

  • Assuming M-grades equal W-grades: they encode different things.
  • Ignoring the induction basis: 1.5 T and 1.7 T are not comparable.
  • Chasing loss alone: B8 induction decides core size.
  • Mixing semi-processed with fully processed: annealing changes the result.
  • Buying thin gauge for low frequency: the premium buys nothing there.

Each trap costs money quietly, and most appear only after the core is built.

A Three-Question Shortcut

Ask what flux direction the machine uses, ask what frequency it runs, then ask what loss the customer will accept. Direction picks the branch, frequency picks the gauge, and tolerance picks the tier. Therefore, three answers narrow dozens of codes to two or three.

Where Families Land in Service

Transformer cores take oriented grades, and the efficiency note explains why their loss matters so much. Motor stators take non-oriented grades, and the applications guide maps the rest.

Silicon steel grade codes printed on a mill test certificate

Frequently Asked Questions

Which grade is the most common?

50W470 for motors, and 27P110 to 30P120 for transformers.

Does a lower trailing number always mean better?

Yes within one family, although price and availability intervene.

Can I substitute M19 for 50W470?

Only after comparing stated loss, never by name alone.

What does the P and W stand for?

P marks oriented grades, and W marks non-oriented ones.

Is 6.5% silicon steel a separate grade family?

Yes, and it trades saturation for resistivity.

What We Do Not Do

  • We do not roll, anneal, or coat steel.
  • We do not convert grade codes between standards.
  • We do not stamp laminations.

Consequently, we quote the code you specify, with its basis stated.

Specify Your Order

  1. State flux direction and frequency.
  2. Name the code, or give the loss limit.
  3. Give gauge and slit width, then confirm tonnage and port.

M36 Non Oriented Electrical Steel covers cost-driven motor builds, and quotes return within one working day.

  • Email: vera.liang@ztwysteel.com
  • Location: Xishan District, Wuxi, Jiangsu, China
  • Supply range: CRNGO M19–M47 at 0.35–0.65 mm, CRGO M4/M5 at 0.23–0.35 mm
  • Slitting: 20–1250 mm, ±0.05 mm, burr under 0.02 mm
  • Documentation: MTC EN 10204 3.1, core loss per ASTM A343 / IEC 60404-2