What thicknesses are available for non-oriented electrical steel?
Five rungs carry most orders, namely 0.35, 0.50, 0.65, 0.80, and 1.00 mm. Two inch-based rungs follow, at 0.47 and 0.64 mm. That thickness range looks narrow, yet it covers nearly every motor built today. Jiangsu Zhongtong Weiye Special Steel Co., Ltd. holds stock at the middle rungs and rolls the rest to order.
Why Thickness Comes in Steps
A mill sets its roll gap for a campaign, so gauge is a schedule decision rather than a dial. Changing gauge mid-campaign wastes a set of rolls, since the pass plan must be rebuilt. Hence mills publish a fixed list, and buyers choose a rung.
Steps save more money than they cost.
The Five Metric Rungs
- 0.35 mm — high-speed and high-efficiency stators
- 0.50 mm — the volume standard for 50 Hz motors
- 0.65 mm — larger frames and slower rotors
- 0.80 mm — heavy industrial machines
- 1.00 mm — low-frequency and structural cores
Each rung matches a band of operating frequency, so the schedule stays short.
The Two Inch Rungs
US practice builds on 0.0187 inch and 0.025 inch, which convert to 0.47 and 0.64 mm. M19 and M36 buyers ask for those gauges by habit, since their drawings predate metrication. Therefore, we keep both conversions on file.
Two systems, one shelf.
The Eddy Arithmetic
Eddy loss follows gauge squared, while hysteresis barely moves with gauge. Dropping from 0.50 to 0.35 mm therefore leaves about 49% of the eddy term. Going from 1.00 to 0.65 mm leaves about 42%. Hence thin rungs matter most where frequency runs high. That is why a 400 Hz machine rarely uses 0.65 mm.
What the Coatings Cost in Fill
A 0.35 mm sheet may carry 0.5 µm of coating on each side. That layer takes a larger share of a thin sheet than of a thick one. Consequently, thin stacks hold less steel per unit height, so the coating spec belongs beside the gauge spec.
Where Thinner Sheet Comes From
Anything below 0.35 mm rolls to order, since mills schedule it for specific customers. Lead time runs six to eight weeks, and the premium sits above stock grades. Consequently, thin sheet belongs in a planned programme, not in a repair order.
Where 0.50 mm Still Wins
Half-millimetre sheet dominates because it balances loss, stacking, and price. Punch shops know its behaviour, so tooling is already set for it. Therefore, prototypes often start there.
Thickness Tolerance
Standard tolerance runs near ±0.05 mm on the middle rungs, while thin sheet tightens further. A stack built on nominal gauge drifts when half the sheets sit at the upper limit. Hence check tolerance before you fix the core window. Most disputes start with a nominal figure, not a real one.
What High-Frequency Machines Need
At 400 Hz, eddy loss dominates and thin sheet pays back quickly. Yet below 0.35 mm, handling damage rises, since the sheet buckles easily. Therefore, high-speed rotors often stop at 0.35 mm.
Stacking Factor Changes With Gauge
Thinner sheet carries a relatively thicker coating, so the stacking factor falls slightly. A 1.00 mm stack reaches higher fill than a 0.35 mm stack of the same height. Therefore, gauge choice alters the magnetic area, not only the loss.
Where the Rungs Come From Historically
Metric rungs follow IEC practice, which fixed the 0.50 mm standard decades ago. Inch rungs follow US practice, where thickness was quoted in thousandths. Consequently, catalogues still show both, and neither is wrong.
What Width Does to Gauge
Narrow slit widths leave more trim per tonne, so a thin, narrow order costs more than its gauge suggests. Wide masters amortise the trim across more strip, which favours stock widths. Hence plan width and gauge together.
What a Thin Campaign Costs the Mill
A thin campaign runs slower, and yield falls as breakage rises. Those costs spread across the tonnage, so small orders pay more per tonne. Hence a full heat is the cheapest way to buy thin sheet.
How to Specify
First, name the operating frequency, since that sets the rung. Second, give the loss class, which sets the grade at that rung. Then state tolerance and width, so the quote matches the drawing.
Three inputs, one rung. Then a buyer can compare quotes without translating rungs.
A Quick Check on a Delivery
Measure ten points per coil with a micrometer, then compare against the certificate. A drift of 0.03 mm across a stack adds up over a thousand laminations. Hence gauge audits belong in incoming inspection.
Related Reading
The grade list is covered in the NGO grades note, and the loss basis appears in the M15 note.
Where Our Stock Sits
We keep 0.50 and 0.65 mm most weeks, since motor shops order them continuously. Thin and heavy rungs come on request. Therefore, urgent repairs usually land on a stock gauge.

Frequently Asked Questions
Yes, and thinner sheet comes to order.
That gauge converts from 0.0187 inch.
Yes at the same frequency, although it stacks better.
Yes, and each coil keeps its own certificate.
Yes, and it serves low-frequency cores.
What We Do Not Do
We do not roll steel, since mills own that step. We do not promise a gauge outside the published list without a campaign. Nor do we quote tolerance as a nominal figure.
Those limits keep the schedule honest.
Specify Your Order
First, state gauge and tolerance. Second, give width and tonnage. Then name the coating, so the laminations behave on your line.
M36 Non-Oriented Electrical Steel covers the 0.64 mm rung. M19 Non-Oriented Electrical Steel serves the 0.47 mm rung. Reactor Core Lamination suits gapped cores at thicker gauges.
- Email: vera.liang@ztwysteel.com
- Location: Xishan District, Wuxi, Jiangsu, China
- Supply range: CRNGO 0.35–1.00 mm in five rungs, thinner classes to order
- Slitting: 20–1250 mm, ±0.05 mm, burr under 0.02 mm
- Documentation: MTC EN 10204 3.1, gauge and tolerance stated per coil