What is the difference between fully processed and semi-processed non-oriented electrical steel?

One sentence carries the whole difference: the last anneal belongs to the mill, or to your plant. Semi-processed coils arrive unannealed, so your furnace finishes the job after punching. Fully processed coils arrive finished, so your press is the last step. Jiangsu Zhongtong Weiye Special Steel Co., Ltd. supplies both states on the same grade.

The One-Line Answer

Fully processed means the mill performed the final anneal and applied the coating. Semi-processed means the mill stopped earlier, leaving carbon in the steel. Consequently, the buyer inherits one process step, and with it, one set of risks.

What the Mill Hands Over

A fully processed coil is annealed, decarburised, and coated, so it is ready to punch and stack. A semi-processed coil is rolled and may carry a light oil, yet it still needs decarburisation. Hence the two coils look similar on a pallet and differ inside.

Why Semi-Processed Exists

Punching strains the grain structure, and that strain raises loss by several percent. Finishing the anneal after punching therefore removes the strain from the finished part. Semi-processed steel exploits that order of operations, so the final lamination carries no punching penalty. That penalty is real, since a punched edge disturbs grains within a millimetre of the cut.

The Order of Operations

Fully processed runs mill anneal, then punching, then assembly. Semi-processed runs rolling, then punching, then your anneal, then assembly. That swap moves the furnace from a steelworks to a motor plant. Consequently, the loss figure on your certificate describes a different stage.

Where the Carbon Comes From

Semi-processed sheet keeps roughly 0.02% to 0.04% carbon, since that carbon eases punching. The final anneal pulls it below 0.005%, which removes magnetic ageing. Hence the furnace does two jobs at once, softening and purifying.

What You Take On With Semi

Five duties arrive with the coil, namely furnace atmosphere, dew point control, soaking temperature, cooling rate, and coating repair. Each duty can ruin a batch if it drifts. Hence semi-processed steel suits plants that already anneal laminations.

What Goes Wrong in an Anneal

A wet atmosphere oxidises the surface, and that oxide blocks interlayer insulation. A short soak leaves carbon in place, which raises loss over time. Therefore, log dew point and soak time for every batch.

Temperatures and Atmospheres

The final anneal usually sits between 780 and 850 °C, in a hydrogen and nitrogen mix. Dew point must stay low enough to pull carbon out, yet not so low that the surface oxidises. Therefore, a dew-point meter belongs beside the furnace controller.

Coating After the Anneal

Annealing strips most organic coatings, so semi-processed parts often need a fresh coat or a bonding varnish. Fully processed parts keep their coating through stamping, which saves that step. Consequently, coating cost lands on one side or the other.

Punching Behaviour

Semi-processed sheet is softer, since the final anneal has not hardened it, so dies wear more slowly. It also burrs less, which helps stacking. Fully processed sheet punches cleanly too, yet its coating must survive the stroke.

Where the Loss Lands

A fully processed 50W470 coil ships at 4.70 W/kg, and punching may add a few percent. A semi-processed coil of similar chemistry can land lower after a good anneal, because the strain is gone. Hence the finished part decides the comparison, not the coil.

Cost Arithmetic

Semi-processed steel sells below fully processed, since the mill skips one anneal. Your plant then pays for gas, electricity, labour, and yield loss. Consequently, the cheaper coil wins only when the furnace runs full. A furnace that runs half empty rarely justifies the cheaper coil.

Which Buyers Choose Which

Hermetic compressor plants often choose semi-processed, because they anneal every part anyway. Large motor builders usually choose fully processed, since they buy laminations ready to stack. Repair shops choose fully processed, because they own no furnace. Small plants sometimes outsource the anneal, which keeps the choice open.

Three cases, three answers.

How to Specify

State the condition on the purchase line: fully processed or semi-processed. Add the annealing cycle if you own that step, so the mill can match chemistry to it. Then confirm the coating, because the anneal may remove it. One clause prevents a shipment of the wrong state.

Where Certification Splits

Fully processed certificates state the loss of the shipped coil. Semi-processed certificates state chemistry, gauge, and a target after anneal. Consequently, the two documents cannot be compared line for line.

Related Reading

The grade list is covered in the NGO grades note, and thickness options appear in the thickness note.

Fully processed and semi-processed non-oriented electrical steel coils side by side

Frequently Asked Questions

Is semi-processed cheaper?

Yes per tonne, although the furnace adds cost.

Can I skip the anneal?

No, since carbon and strain would remain.

Does fully processed need annealing after punching?

Only for tight loss targets.

Which state suits a repair shop?

Fully processed, since no furnace is available.

Can both states share one grade code?

Yes, and the condition is stated separately.

What We Do Not Do

We do not anneal laminations for customers. We do not sell semi-processed sheet as ready to use. Nor do we promise a loss figure before the final anneal.

Those limits keep the two states distinct.

Specify Your Order

First, state the condition you need. Second, give grade, gauge, and width. Then name the coating, so the finished part behaves as planned.

M36 Non-Oriented Electrical Steel ships fully processed. M19 Non-Oriented Electrical Steel covers the M19 class. Reactor Core Lamination serves gapped cores.

  • Email: vera.liang@ztwysteel.com
  • Location: Xishan District, Wuxi, Jiangsu, China
  • Supply range: CRNGO 0.35–1.00 mm, fully or semi-processed
  • Slitting: 20–1250 mm, ±0.05 mm, burr under 0.02 mm
  • Documentation: MTC EN 10204 3.1, condition and loss basis stated per coil