How High Precision Silicon Steel Sheet Cuts Down Post-Processing Waste

Precision silicon steel sheet saves money after it leaves the mill. Full-width coil needs slitting, deburring, and flattening before stamping. Consequently, tight tolerance upstream means less work downstream. At Jiangsu Zhongtong Weiye Special Steel Co., Ltd., we slit to ±0.05 mm. Here is how that cuts waste.

Where Post-Processing Waste Comes From

Source Typical waste Fix
Width out of tolerance 5–10% trim Slit to ±0.05 mm
Edge burr 2–5% rework Precision slitting
Wavy strip 3–5% scrap Tension leveling
Thickness variation 1–3% lamination factor loss Mill tolerance control
Oil on surface Stamping downtime Clean, controlled coating

Lever 1: Tight Slit Width

Standard slitting holds ±0.20 mm. Consequently, a stator shop must trim to final width. We slit to ±0.05 mm. Furthermore, the strip feeds the progressive die without trimming. Consequently, scrap drops by 5–10% per stamped part.

Lever 2: Burr-Free Edge

A burr on the strip edge catches in the die. Furthermore, it creates short circuits between laminations. Consequently, we control slitting clearance and shear angle. The result: burr height under 0.02 mm. Consequently, no deburring needed before stacking.

Lever 3: Flatness

Wavy strip does not feed evenly. Furthermore, it causes uneven stack height. Consequently, we tension-level coil before slitting. The strip lies flat on the press. Consequently, the stator stacks to the correct height without shimming.

Lever 4: Consistent Thickness

Thickness variation drops the lamination factor. A 1% thickness spread means 1% less iron in the core. Furthermore, that 1% raises core loss. Consequently, we hold thickness to ±0.01 mm. The result: higher lamination factor and lower loss.

The Math for a Motor Shop

Suppose you stamp 1 million stators per year. If each stator saves 5 grams of trim: that is 5 tons of scrap avoided. Furthermore, deburring labor drops. Consequently, tight tolerance pays back in months.

What We Supply

We ship precision-slit electrical steel:

  • CRNGO: M19, M27, M36, M43.
  • CRGO: 27QG110, 30Q120.
  • Slit width tolerance: ±0.05 mm.
  • Thickness tolerance: ±0.01 mm.
  • Coil ID: 508 mm or 406 mm.

Furthermore, we pack for ocean freight with VCI paper.

precision silicon steel sheet

What We Do Not Do

We do not:

  • Stamp finished laminations.
  • Run progressive dies.
  • Supply amorphous metal cores.

Consequently, we are your upstream precision-slit coil supplier.

Specify Your Precision Requirements

Tell us:

  1. Required slit width and tolerance.
  2. Thickness and grade.
  3. Burr height limit.
  4. Annual volume.

We will confirm our capability and quote.

  • Email: vera.liang@ztwysteel.com
  • Location: Xishan District, Wuxi, Jiangsu, China
  • Supply range: CRNGO non-oriented steel, CRGO grain-oriented steel, precision-slit strip
  • Tolerances: slit width ±0.05 mm, thickness ±0.01 mm, burr <0.02 mm
  • Documentation: MTC with core loss, thickness, width, and coating

We reply within one working day.