Causes and Preventive Measures for Coating Peeling Problems
Coating peeling wastes more money than any other surface-finish failure. The paint looks fine at acceptance, then lifts off within months. Consequently, the root cause almost always sits in surface preparation, not the paint itself. Here are the five most common causes and the fix for each.
Cause 1: Surface Contamination
Oil, grease, drawing compound, or fingerprints block adhesion. The paint bonds to the oil film, not the metal. Consequently, when the oil migrates, the paint lifts off.
Fix: Degrease before coating. Use alkaline cleaning or solvent wipe. Furthermore, do not touch the cleaned surface with bare hands. For tinplate can stock, specify “lacquer-ready” oil weight (8–12 mg/m² palm oil), not heavy rust-preventive oil.
Cause 2: Inadequate Surface Roughness
A mirror-smooth surface gives paint nothing to grip. Conversely, too much roughness traps air under the coating. Consequently, the correct profile matters.
Fix: Abrade or blast to the specified roughness. For paint on steel, Sa 2.5 blast profile (50–75 μm) is standard. For lacquer on tinplate, the stone finish from temper rolling is sufficient.

Cause 3: Incompatible Coating System
Paint chemistry must match the substrate. Epoxy does not bond well to galvanized steel without a primer. Furthermore, two paint layers of incompatible chemistry delaminate from each other.
Fix: Use the primer system the paint manufacturer recommends. For tinplate food cans, epoxy phenolic lacquer is standard on both sides. For external can decoration, use UV-cured ink or varnish over base coat.
Cause 4: Thermal Expansion Mismatch
Metal and coating expand at different rates. When temperature cycles, the coating shears away from the substrate. Consequently, parts that see wide temperature swings peel first.
Fix: Use flexible coatings that stretch with the substrate. Furthermore, avoid thick films—thick coatings crack more easily. For outdoor steel structures, use elastomeric or acrylic latex coatings rated for thermal movement.
Cause 5: Chemical or UV Attack
Solvents, acids, and sunlight break down the coating’s chemical bonds. Consequently, coatings on outdoor equipment or chemical service fail faster.
Fix: Specify the coating for the service environment. For chemical exposure, use epoxy or polyurethane. For outdoor UV exposure, add a polyurethane topcoat. Furthermore, inspect and touch up damaged areas before rust forms.
Related Products Where Coating Adhesion Matters
We supply substrates that fabricators then coat or lacquer:
- C11000 / T2 Copper Plate ships clean and PVC-film protected, ready for painting or powder coating.
- C12200 / TP2 Copper Tube gets internal cleaning before end caps are applied.
- H13 / SKD61 Mold Steel arrives soft-annealed and machinable, ready for nitriding or PVD coating.
Prevent Peeling Before It Happens
Tell us your substrate and intended coating system. We will confirm surface condition and packing to give your coater the best starting point.
- Email: vera.liang@ztwysteel.com
- Location: Xishan District, Wuxi, Jiangsu, China