What mold steel should I choose for plastic injection molds?

Start with the cavity surface, since plastic injection mold steel follows the finish you must deliver. A textured housing, a high-gloss lens, and a glass-filled bracket each need a different grade. Jiangsu Zhongtong Weiye Special Steel Co., Ltd. stocks the four conditions these tools usually need.

The Default: A Pre-Hardened P20 Type

Most tools begin with a 30 to 34 HRC pre-hardened plate, and 1.2311 fills that role. It machines easily, holds a polish, and needs no heat cycle. Hence roughly seven out of ten new moulds start there.

Demand 1 — High Gloss Surfaces

A mirror face exposes every inclusion, so the steel must be clean rather than hard. Low-sulphur, low-inclusion plate at 30 to 34 HRC polishes without comet tails. Therefore, lens and cosmetic tools often specify an ESR or vacuum-melted grade.

Demand 2 — Etched Textures

Texture etching attacks hardness differences, since acid bites the softer phase faster. A banded plate therefore etches unevenly and shows streaks. A 30 to 34 HRC block etches cleanly across the whole face. Hence texture work needs uniform hardness through the block.

Demand 3 — Glass-Filled Resin

Glass fibre at 20 to 30% by weight grinds a soft cavity, so a P20 face wears within months. A hardened insert at 48 to 52 HRC resists that abrasion. Consequently, glass-filled parts usually run hardened inserts in a soft holder.

Demand 4 — Corrosive Resin

PVC releases hydrogen chloride, which condenses into acid on a cool face. POM releases formaldehyde at high melt temperature. Both attack plain alloy steel, so 4Cr13H at 13% chromium suits those resins.

Demand 5 — Very Large Moulds

A block above roughly 400 mm thick hardens unevenly, since a plain P20 grade loses hardness at the centre. Nickel at about 1% improves through-thickness response, which is what 1.2738 provides. Hence large appliance and automotive tools often use that grade.

Demand 6 — Very Long Runs

Above one million shots, even a hardened face begins to wear at the gate. A changeable insert at 58 to 62 HRC, such as a D2-type steel, protects the expensive block behind it. Therefore, high-volume tools are designed around replaceable inserts. Such inserts also shorten a repair from weeks to days.

How Many Cavities Change the Answer

A single-cavity tool can use one block, since balance is not a problem. A 32-cavity tool needs identical hardness across all cores, or filling drifts. Hence multi-cavity work favours a through-hardening grade.

Why Wall Thickness Matters

A thin core cools fast, while a thick boss stays hot for minutes. That heat soak softens a pre-hardened face over time. Consequently, thick bosses often take a harder insert than the surrounding cavity.

What Surface Treatment Adds

Nitriding is rarely used on plastic moulds, since it dulls a polish. Hard chrome protects a textured face instead. Hence coatings belong on wear zones, not on gloss.

Free-Cutting Variants

Sulphur added to a P20 type improves machinability, which is what 1.2312 offers. The trade-off is lower polish quality, since sulphide stringers show on a mirror face. Those stringers also reduce toughness across the grain. Hence free-cutting plate suits structural parts, not visible ones.

Why Stress Relief Comes First

Rough machining leaves stress in a thick block, so the cavity can move during finishing. A stress-relief cycle near 500 °C removes most of it. Therefore, plan the relief before the final cut.

The Price Ladder

Annealed plate costs least, then pre-hardened, then ESR pre-hardened, then hardened tool steel. Each step buys either finish or life, not both. Therefore, pay for the property your product actually needs.

What a Tool Room Checks on Arrival

Ultrasonic testing finds internal cracks, which a hard face would hide. Hardness mapping finds soft spots in a thick section. Hence both checks belong before the first cut.

What the Drawing Should Say

Name the grade and the delivery hardness, then the polish or etch requirement. Add the resin and any filler content, since that sets the wear rate. Finally, state the block size, so the hardenability matches the section.

When Annealed Plate Is the Right Buy

A shop with its own furnace may prefer annealed stock, since it controls the cycle. The block then hardens to the exact section need. Therefore, in-house heat treatment changes the buying decision.

Related Reading

The gloss-versus-corrosion choice appears in the 4Cr13H note, and the family sits in the mould steel note.

Pre-hardened P20 type plate being milled for a plastic injection mold cavity

Frequently Asked Questions

Is 1.2311 the same as P20?

Close, since both sit near 30 to 34 HRC pre-hardened.

Which grade for a glossy lens tool?

A low-inclusion pre-hardened plate, often ESR.

Do glass-filled parts need H13?

Often yes, since abrasion removes a soft face quickly.

When do I need 1.2738?

Above roughly 400 mm thickness, for even hardness.

Can one block cover all demands?

Rarely, and inserts let one tool use two grades.

What We Do Not Do

We do not polish, etch, or heat-treat blocks. We do not promise a mirror finish from any grade. Nor do we sell free-cutting plate for visible surfaces.

Those limits keep the advice usable.

Specify Your Order

First, name the grade and the condition. Second, give thickness, width, and length. Then state the finish and the resin, so the plate matches the cavity plan.

4Cr13H Plastic Mould Steel covers corrosive resins. H13 Tool Steel 1.2344 covers hardened inserts. D2 Cold-Work Steel covers long-run wear.

  • Email: vera.liang@ztwysteel.com
  • Location: Xishan District, Wuxi, Jiangsu, China
  • Supply range: pre-hardened plate 30–34 HRC, 12–400 mm; hardened tool steel on request
  • Cutting: length under 4 m, ±1 mm, squareness 1 mm per metre
  • Documentation: MTC EN 10204 3.1, hardness and inclusion class stated per plate