Precision in Every Cut: The Engineering Behind Custom Silicon Steel Laminations
Silicon steel laminations decide core performance at the edge. A stamping die cuts thousands of parts per hour. Furthermore, every cut introduces mechanical stress at the sheared edge. If the strip is inconsistent, that stress ruins magnetic properties. At Jiangsu Zhongtong Weiye Special Steel Co., Ltd., we supply the precision-slit strip that makes clean stamping possible. Here is what matters.
How Cutting Affects Magnetic Performance
When you shear electrical steel:
- The edge work-hardens and distorts.
- Magnetic domains near the edge misalign.
- Permeability drops locally.
- Core loss rises 5–15% near the cut edge.
Consequently, a clean, controlled cut preserves magnetic properties. A dull die or wrong clearance ruins them.
The Three Strip Quality Factors
| Factor | Target | Effect if off |
|---|---|---|
| Slit width | ±0.05 mm | Die jams, poor fit |
| Burr height | <0.02 mm | Short circuits between laminations |
| Flatness | <0.1 mm wave | Poor stack, air gaps |
Why Burr Matters
A burr on the lamination edge pierces the insulation coating. Furthermore, adjacent laminations short-circuit through the burr. Consequently, eddy current loops grow across the stack. The core heats up. Consequently, we control slitting clearance to keep burr under 0.02 mm.

Why Stack Factor Matters
Stack factor = (iron height) / (total stack height). A 95% stack factor means 5% air. Furthermore, air gaps raise magnetic reluctance. Consequently, the transformer or motor needs more magnetizing current. Tight thickness tolerance and low burr hold stack factor above 96%.
What We Supply
We ship precision-slit electrical steel:
- CRNGO: M19, M27, M36, M43.
- CRGO: 27QG110, 30Q120.
- Slit width tolerance: ±0.05 mm.
- Burr height: <0.02 mm.
- Coil ID: 508 mm or 406 mm.
Furthermore, we pack for ocean freight with VCI paper.
What We Do Not Do
We do not:
- Stamp finished laminations.
- Run progressive dies.
- Build transformer or motor cores.
Consequently, we are your upstream precision-slit coil supplier for stamping shops.
Specify Your Lamination Strip
Tell us:
- Stator or lamination geometry.
- Required slit width and tolerance.
- Burr height limit.
- Annual volume.
We will confirm our capability and quote.
- Email: vera.liang@ztwysteel.com
- Location: Xishan District, Wuxi, Jiangsu, China
- Supply range: CRNGO non-oriented steel, CRGO grain-oriented steel, precision-slit strip
- Tolerances: slit width ±0.05 mm, burr <0.02 mm, thickness ±0.01 mm
- Documentation: MTC with core loss, thickness, width, and coating
We reply within one working day.